NOTE |
DESCRIPTION |
DIAMETER INCHES |
TENSION LBS |
1st G |
Cryogenic Stainless Steel Wound |
.045 |
|
2nd D |
Cryogenic Stainless Steel Wound |
.065 |
|
3rd A |
Cryogenic Stainless Steel Wound |
.085 |
|
4th E |
Cryogenic Stainless Steel Wound |
.105 |
|
4th B |
Cryogenic Stainless Steel Wound |
.125 |
|
Cryogenic -320 strings are bathed in liquid nitrogen to -320F. The process removes residual stresses in the crystalline structure of the high carbon steel core wire. The result is a wire with reduced elasticity, longer life, and improved tuning stability.